Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Styrolution® PS 495N - PS-I - INEOS Styrolution

Material Data Center offers the following functions for Styrolution® PS 495N:
unit conversion, PDF datasheet print, comparison with other plastics, flow length calculation, snap fit calculation, beam deflection calculation, cooling time calculation, parameters for material models, CAE Interfaces

Check here, which other Styrolution PS datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
材料文字说明
Styrolution® PS 495N is a high flow, high impact polystyrene with a good heat resistance and a high stiffness.
加工/物理特性价值单位Test Standard
ISO数据
熔体体积流动速度, MVR 9.5 cm³/10min ISO 1133
温度 200 °C -
载荷 5 kg -
熔体密度 935 kg/m³ -
熔体 0.165 W/(m K) -
熔体的比热 2290 J/(kg K) -
喷射温度 88 °C -
机械性能价值单位Test Standard
ISO数据
拉伸模量 2000 MPa ISO 527
屈服应力 26 MPa ISO 527
屈服伸长率 1.5 % ISO 527
名义断裂伸长率 40 % ISO 527
无缺口简支梁冲击强度, +23°C N kJ/m² ISO 179/1eU
简支梁冲击强度, -30°C 130 kJ/m² ISO 179/1eU
简支梁缺口冲击强度, +23°C 17 kJ/m² ISO 179/1eA
热性能价值单位Test Standard
ISO数据
热变形温度, 1.80 MPa 85 °C ISO 75-1/-2
热变形温度, 0.45 MPa 89 °C ISO 75-1/-2
维卡软化温度, B 88.5 °C ISO 306
线性热膨胀系数, 平行 100 E-6/K ISO 11359-1/-2
1.5mm名义厚度时的燃烧性 HB class IEC 60695-11-10
厚度为h时的燃烧性 HB class IEC 60695-11-10
测试用试样的厚度 3.0 mm -
电性能价值单位Test Standard
ISO数据
相对介电常数., 100Hz 2.5 - IEC 62631-2-1
相对介电常数., 1MHz 2.5 - IEC 62631-2-1
介质损耗因子, 100Hz 4 E-4 IEC 62631-2-1
介质损耗因子, 1MHz 4 E-4 IEC 62631-2-1
相对漏电起痕指数 500 - IEC 60112
其它性能价值单位Test Standard
密度 1030 kg/m³ ISO 1183
函数
粘度-剪切速度 , Styrolution® PS 495N, PS-I, INEOS Styrolution
剪切应力-剪切速度 , Styrolution® PS 495N, PS-I, INEOS Styrolution
应力-应变.  , Styrolution® PS 495N, PS-I, INEOS Styrolution
正割模量-应变.  , Styrolution® PS 495N, PS-I, INEOS Styrolution
比容-温度(pvT) , Styrolution® PS 495N, PS-I, INEOS Styrolution
拉伸模量-温度 , Styrolution® PS 495N, PS-I, INEOS Styrolution
典型数据
加工方法
注塑
特殊性能
高冲击韧性的/经抗冲改性的
地区供应
其他信息
注塑成型
PROCESSING
injection molding, Melt temperature, range: 180 - 260 °C
injection molding, Melt temperature, recommended: 220 °C
injection molding, Mold temperature, range: 10 - 60 °C
injection molding, Mold temperature, recommended: 40 °C

Polystyrol 495N can be injection moulded under different conditions depending on machinery available and articles moulded. Mass temperature can be as high as 260°C. Polystyrol 495N is suitable for gas assisted injection moulding.
权利义务的法律声明
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.